Properties | Metric | Imperial |
Density | 10.3g/cm³ | 0.369lb/in |
Melting point | 2625℃ | 4760℉ |
Properties | Metric | Imperial |
Tensile strength (annealed) |
324 MPa |
47000 psi |
Shear strength (torsional strain rate 0.25/s) |
500 MPa |
72500 psi |
Compressive yield strength (0.01% yield) |
400 MPa |
58000 psi |
Modulus of elasticity |
330 GPa |
47900 ksi |
Modulus of elasticity at elevated temperature (@2000°C/3630°F) |
160 GPa |
23200 ksi |
Thermal Coefficient of Expansion: |
5 x 10-6 cm/cm @ 25 oC |
|
Electrical Conductivity: |
34% I.A.C.S. |
|
Thermal Conductivity: |
1.38 W/cm/K @ 298.2 K |
|
Electrical Resistivity: |
5.2 microhm-cm @ 0 oC |